Spring Fit-Out Checklist for GRP Boats: Cover to Launch

A GRP boat forgives a lot over winter, but spring is when small gelcoat cracks, tired seals and a lazy engine start turn into season-long problems. Work through this checklist in order and she goes back in ready to use, with the gelcoat protected and nothing left to chance on launch day.

White fibreglass motor cruiser on a steel cradle in a spring boatyard with her cover half off, polished gelcoat and fresh blue antifouling

Tools and materials

  • •Hose, soft brush and boat shampoo
  • •Cutting compound, polish and wax
  • •Antifouling and roller
  • •Gelcoat repair kit
  • •Fresh engine oil, filters and impeller
  • •Multimeter and battery charger
  • •Potable-water sanitizer tablets
  • •Marine sealant (MS polymer)

1. Uncover and inspect

Take the cover off on a dry day, clean it and store it dry so it doesn't mildew. Check underneath for standing water, mould on cushions and headlinings, and nests in vents.

Check the cradle pads or trailer bunks are bearing evenly. A hull resting on one pad all winter can show a dent or stress cracks around it.

Open every locker and hatch to air her through, and pump or sponge out any bilge water — note where it came from.

Read the full guide

Sign up free to read the remaining 5 steps. 30-day free trial, no card needed.

Frequently asked questions

How do I tell if my GRP boat has osmosis?

Look for blisters below the waterline after hauling out. Blisters that weep fluid with a vinegar-like smell when pricked are a strong sign. A surveyor's moisture meter reading after the hull has dried for a few weeks gives a proper answer before you decide on treatment.

Should I polish or wax my gelcoat in spring?

Both if the gelcoat is chalky: cutting compound removes the dull oxidised layer, polish brings back the shine, and wax protects it. If the hull is still glossy, a wash and a coat of wax is enough.

Can I put new antifouling over the old?

Yes, if they are compatible. Eroding over hard antifouling usually works after a light key; hard over eroding often flakes off. If you don't know what is on there, use a primer or tie-coat recommended by the paint maker.

How long before launch should I start?

Start four to six weeks before your planned launch date, once the hard frosts are over, so antifouling and gelcoat repairs have time to cure.

Advice here is general guidance only — see our disclaimer. Need a professional? Browse local trades.